Europese norm I-profielen
Flens helling: 14%
Afmeting:
IPN 80 - IPN 550 DIN 1025-1: 1995, NF A 45-209: 1983
IPN 600 DIN 1025-1: 1963
Toleranties:
EN 10024: 1995
Oppervlaktegesteldheid:
Volgens EN 10163-3: 2004, klasse C, subklasse 1
Benaming | Afmeting | A mm2 ( x102) |
Afmetingen voor Detaillering | |||||||||
G kg/m |
h mm |
b mm |
tw mm |
tf mm |
r1 mm |
r2 mm |
d mm |
o | Pmin mm |
Pmax mm |
||
IPN 80 | 5.94 | 80 | 42 | 3.9 | 5.9 | 3.9 | 2.3 | 7.58 | 59 | - | - | - |
IPN 100 | 8.3 | 100 | 50 | 4.5 | 6.8 | 4.5 | 2.7 | 10.6 | 75.7 | - | - | - |
IPN 120 | 11.1 | 120 | 58 | 5.1 | 7.7 | 5.1 | 3.1 | 14.2 | 92.4 | - | - | - |
IPN 140 | 14.3 | 140 | 66 | 5.7 | 8.6 | 5.7 | 3.4 | 18.3 | 109.1 | - | - | - |
IPN 160 | 17.9 | 160 | 74 | 6.3 | 9.5 | 6.3 | 3.8 | 22.8 | 125.8 | - | - | - |
IPN 180 | 21.9 | 180 | 82 | 6.9 | 10.4 | 6.9 | 4.1 | 27.9 | 142.4 | - | - | - |
IPN 200 | 26.2 | 200 | 90 | 7.5 |